Embrace the exquisite beauty of Chequered Plywood, transforming your space into a haven of elegance.
The Art Deco Era movement in the 1920s and 1930s had a significant role in the development of chequered plywood as this era witnessed the growth of the utilization of geometric patterns on the plywood. The structural integrity of this plywood is also thankful for the advancement of the plywood manufacturing process which bloomed in the 19th century.
What is the difference between chequered plywood and pre-laminated plywood? In the case of chequered plywood, the pattern is engraved on its surface whereas in the case of pre-laminated, a thin sheet of laminate is glued on the top of the plywood.
This chequered plywood is highly used in the area which demands anti-slipping properties as its surface is rigid. It is mostly used as a flooring material.
Chopra’s chequered plywood has load-bearing capacity due to extra compression techniques and is impregnated with RPF resins, which is a type of resin that is used to enhance performance and increase its utility in various applications. Impregnating with RPF resins holds 30% of the overall weight of the plywood.
TECHNICAL SPECIFICATION [AS:315:64:2010] | |||||
S.NO | DIMENSIONS | BIS REQUIREMENTS | OBSERVED VALUES | ||
1 | Length |
|
2442mm | ||
2 | Width |
|
1222mm | ||
3 | Thickness | 12mm | 11.90mm | ||
4 | Squareness | 2mm/1000mm | 0.55mm | ||
5 | Edge Straightness | 2mm/1000mm | 0.50mm | ||
6 | Workmanship & finish | Clause | Satisfactory | ||
Physical Properties | |||||
7 | Density | 0.84 | 0.867 | ||
8 | Moisture Content | 5-15% | 6.80% | ||
9 | Bond Quatlity Test Boiling – Drying @ 60+_2°c 4 Hrs. – 20 Hrs. Three Cycles |
a) No Visible delamination in glue line and plywood face b) No forcible separation and fibre should be adhered between plies |
Satisfactory Satisfactory |
||
10 | Breaking Strength 250 x 50 x Thickness(mm) |
200kgf | 220kgf | ||
11 | Static Bending Strength Along the grain M.O.E. Across the grain M.O.E. Along the grain M.O.R. Across the grain M.O.R. |
Avg. -7500N/mm² Ind. – 6700N/mm² Avg. – 4000N/mm² Ind. – 3600N/mm² Avg. – 50N Ind. – 45 Avg. – 30 Ind. – 27 |
18528.32N/mm² 12620.25N/mm² 15308.24N/mm² 9415.78N/mm² 100.81N/mm² 75.32N/mm² 85.39N/mm² 67.86N/mm² |
||
12 | Tensile Strength as per ASRTU |
|
568kg/cm² 495kg/cm² 1063kg/cm² |